GH4169 N07718 Inconel 718 nickel strip superalloy coil

FOB Reference Price : Get Latest Price


title :

GH4169 N07718 Inconel 718 nickel strip superalloy coil

Type :

coil

Material :
stainless steel, carbon steel, galvanized, aluminum, copper, alloy steel

Contact us :
Contact us for a quote

Email :
contact@asiametalltd.com (your request will be responsed within 1 hour.)

Inconel718 alloy is a precipitation hardening nickel chromium iron alloy containing niobium and molybdenum. It has high strength, good toughness and corrosion resistance at 650 ℃. Its state can be solution treatment or precipitation hardening.

 

 

Product Name

Bright finished GH4169 N07718 Inconel 718 nickel strip superalloy coil

Standard

ASTM, AISI, GB, JIS, EN, DIN

Specification

Width: 500~1500mm

Thickness: 0.2~8.0mm

Length: 50m~100m

Type

Cold/Hot rolled plate, thick plate, color coated plate, galvanized plate

Nearly Brand

GH4169, UNS N07718, DIN 2.4668, NC19FeNb, NiCr19Nb5Mo3(ISO)

Quality

MTC

Package

Standard seaworthy package or Customized.

Delivery Time

5-30 working days after receiving the down payment.

*Payment Term

Trade assurance, Western Union, L/C, etc

By T/T, 50% down payment, 50% balance before shipment.

 

Physical properties

 

-196℃

20℃

100℃

500℃

1000℃

Modulus of elasticity (Gpa)

       

28.27

Mean coefficient of thermal expansion

   

198.57

110.0

99.0

Coefficient of heat conduction (w/m℃)

         

Specific heat capacity (j/kg.℃)

5.9

       

Than the resistance (Ωmm2/m)

       

1.35

 

 

Density

8.4g/cm3

Tensile strength σb (MPa)

≥965

Elongation δ5 (%)

≥30

Yield Strength σs (MPa)

≥550

Brinell hardness (HB)

≤363

 

20201102170119.jpg

 