Parameters | Specification |
Type | Inconel X-750 |
Chemical Composition | Ni:70%,Cr:16% |
Max continue operating temp.(°C) | 1425 |
Density at 20 °C (g/cm3) | 8.25 |
Elongation % | 30 |
Min tensile strength in N/mm2 | 930 |
Inconel X-750 process performance and requirements:
1.The forging temperature of the alloy is easy to form between 1220 and 950 °C.
2.The alloy is fixed and treated after intense forming process.
3.The average grain size of the alloy is closely related to the deformation degree and final forging temperature.
4, the alloy has a good welding performance, can carry on a variety of welding. After welding, the strength of the approximate complete heat treatment state can be obtained by aging treatment.
5.Heat treatment of parts is carried out in a neutral or reducing atmosphere without sulfur to avoid vulcanization.